  浴缸處理前之外貌
嚴重崩爛
Cart-iron and steel tubs with porcelain surfaces can
become thin and porous over time. This leads to pin
holes, rust, chip and exposed metal areas.

 

 

  經過特制堅硬補理
把崩爛的地方補回原狀
Chip, cracks and dings are repaired and refilled.

 

 

  經過化學原料處理
浴缸表面污漬及粗糙化
The entire area is prepared for treatment. It ensures
the coating is applied only to the proper surface and
that no oversprary damage to any other surface.

 

 

  經過工具噴塗,再造(瓷釉塗料底層)
再用高溫烘乾
A Chemical bonding agent / printer, provides a bond
between the surface and the costing.

 

 

  經過磨沙處理底層表面的塵粒以至光滑乾淨
再造(面層)
Refining and Surfacing the bathtub.

 

 

  除去報紙及清潔浴室令嚴重崩爛的浴缸徹底變新
光滑明亮 完整無缺
After drying, it's a whole new look for the bathtub,
a brilliant shining surface.

 

 

 